Reasons to buy steel square in Georgia from the manufacturer

Alloy 426 / UNS K94660 / 1.3926 / Ni42Cr6

📄 Product Description: Alloy 426 — Heat-Resistant and Corrosion-Resistant Iron-Based Alloy with Chromium and Nickel 🧾 General Technical Characteristics Alloy 426 is a heat-resistant, iron-based alloy with a high chromium content (~26%) and moderate nickel content (~8%), developed for use in high-temperature environments and aggressive atmospheres. It offers excellent oxidation resistance, strong mechanical performance at […]

Description

📄 Product Description: Alloy 426 — Heat-Resistant and Corrosion-Resistant Iron-Based Alloy with Chromium and Nickel

🧾 General Technical Characteristics

Alloy 426 is a heat-resistant, iron-based alloy with a high chromium content (~26%) and moderate nickel content (~8%), developed for use in high-temperature environments and aggressive atmospheres. It offers excellent oxidation resistance, strong mechanical performance at elevated temperatures, and good weldability.

It is ideally suited for components operating under thermal and mechanical stress, including furnace elements, heat exchangers, exhaust systems, and power generation equipment.

⚙️ Applications

  • Heat exchangers and piping
  • Combustion chambers and industrial furnace parts
  • Turbine casings
  • Exhaust system components
  • Chemical processing equipment

📈 Key Advantages

  • ✅ Oxidation resistance at high temperatures up to 1100 °C
  • ✅ Good mechanical strength under heat
  • ✅ Corrosion resistance in aggressive environments
  • ✅ Excellent weldability
  • ✅ Durability under cyclic thermal loading

🧪 Chemical Composition (typical for Alloy 426)

Element Content (%)
Iron (Fe) Balance
Chromium (Cr) ~25–27
Nickel (Ni) ~7–9
Molybdenum (Mo) ≤ 1.0
Carbon (C) ≤ 0.05
Manganese (Mn) ≤ 1.0
Silicon (Si) ≤ 1.0
Nitrogen (N) ≤ 0.10

🧩 Mechanical and Physical Properties

  • Tensile Strength: ~500–750 MPa
  • Yield Strength: ~250–400 MPa
  • Elongation: ≥ 25%
  • Hardness: ~170–220 HB
  • Density: ~7.7 g/cm³
  • Operating Temperature: up to 1100 °C

✅ Conclusion

Alloy 426 is a high-temperature, corrosion-resistant alloy ideal for use in thermally and chemically demanding environments. It is widely used in power generation, metallurgy, furnace equipment, and other industries where high heat resistance and durability are essential.

Available in sheets, tubes, rods, forgings, and custom-machined parts. Can be supplied in heat-treated condition upon request.

 Delivery Forms Alloy 426

Alloy 426 wheel

Diameter 4-300mm

Alloy 426 sheet

Thickness 0.5-20mm

Alloy 426 Tape

Thickness 0.2-2mm

Alloy 426 strip

Thickness 10-50mm

Alloy 426 wire

Diameter 0.5-9mm

Alloy 426 Tube

– Hot Rolled Round Tube

diameter 38 or more up to 244.5 mm,

thickness from 3 to 25 mm

-Cold drawn round tube

diameter from 6 to 219.1mm

thickness from 0.9 to 14.2mm

Reviews Alloy 426 / UNS K94660 / 1.3926 / Ni42Cr6

There are no reviews yet.

Leave a review Alloy 426 / UNS K94660 / 1.3926 / Ni42Cr6

Viewed products

Similar products

With this product they buy

©2025. Aspersteel. All rights reserved.